Casting Molded Polyurethane Part, PU Part
It consists of A&B component, A is polyol, and B is Hydroxyl-Terminated polyurethane prepolymer.
Product Introduction
We rely on the continuous development of the company, so that all employees in both material and spiritual satisfaction, while continuing to contribute to the development of the social plastic packaging 7 Crystal Water Zinc Borate, PTMEG Type MDI System Polyurethane Elastomer, Two Componment MDI Based Polyurethane Prepolyer industry. We seek and develop the most suitable market for us through a series of methods and strive to achieve the highest share. We constantly meet the needs of our customers, create value and benefits for them, and grow together with them. We strive to create a united, harmonious, relaxed and upward working atmosphere, forming a new corporate culture of innovation and excellence. We are based on long-term, the pursuit of harmony, and strive to achieve coordinated development with partners, customers, society and the environment.
Cold casting two componment Polyurethane
- Composition: It consists of A&B component, A is polyol, and B is Hydroxyl-Terminated polyurethane prepolymer.
- Characteristics: It has excellent processing properties, solid in common temperature, shorter gel time, and regulating colours by adding pigment. The ware has good properties of abrasive resistance, hydrolysis resistance, transparent, good resilience, stable dimension.
- Product application: Rod and bar, sheet and plate, industrial wheel, construction mold, sports equipment coating, skateboard wheel, buffer insole and other polyurethane miscellaneous parts.
- Operation details: After vacuum degassing for the two components (A and B), they are mixing, pouring and casting in mold in proportion at room temperature of 30-40 ℃, it can be used for manual operation and mechanical molding.
- Storage: Store in a cool and dry place and use up as soon as possible after opening; It cannot be used up at one time, and it needs to be replaced with nitrogen and sealed; The secondary opening shall be used for defoaming, and the original storage period is six months.
Item | Type | |||
HJ1885-1 | HJ1880-2AB | HJ1890-2AB | HJ3155 | |
NCO CONTENT % | 8.5±0.2 | 9.0±0.2 | 12.0±0.2 | ------ |
Density 25℃(g/cm³) | 1.10 | 1.10 | 1.10 | 1.23 |
Gel Time /min | 2-3 | 8-14 | 6-9 | 120-150 |
Mixing Ratio A:B | 100:100 | 100:100 | 100:100 | 100:6.4 |
Physical Properties | ||||
Hardness (Shore A) | 85±2 | 82±2 | 90±2 | 55±3 |
Tensile Strength (Mpa) | 10-15 | 9-14 | 18-25 | 20-25 |
Elongation at Break (%) | 350-500 | 350-550 | 400-550 | 450-600 |
Tear Strength (KN/m) | 40-50 | 50-60 | 70-85 | 30-35 |
Compression permanent deformation % | 12-16 | 15-18 | 10-15 | 10-15 |
DIN Abrasion loss(mm³) | ≤120 | ≤120 | ≤120 | ------ |
Resilience %/25℃ | 48-52 | 36-40 | 35-38 | 26-30 |
A | Type | HJ1850A-2 | HJ1860A-2 | HJ1870A-2 |
Appearance(35℃) | colorless viscous liquid | |||
B | Type | HJ1850B-2 | HJ1860B-2 | HJ1870B-2 |
Appearance (35℃) | light yellow viscous liquid | |||
Mixing Ratio A:B | 1:1 | 1:1 | 1:1 | |
Operating temperature (℃) | 35-40 | 35-40 | 35-40 | |
Gel Time (min) | 30-40 | 25-35 | 20-30 | |
Hardness (Shore A) | 50±3 | 60±3. | 70±3 | |
Tensile Strength (Mpa) | 4-6 | 5-8 | 8-10 | |
Elongation at Break (%) | 400-500 | 300-400 | 250-350 | |
Tear Strength (KN/m) | 18-22 | 20-25 | 26-30 | |
Resilience %/25℃ | 30-35 | 30-35 | 30-35 | |
Density 25℃(g/cm³) | 1.17 | 1.17 | 1.17 | |
We are committed to innovation, manufacturing new and excellent Casting Molded Polyurethane Part, PU Part and strive to provide customers with effective solutions. We aim at the forefront of the industry with the global perspective and seize the highest position of the industry. We take the customer as the center, establish the "standardized, orderly and controllable" multi-level after-sales service for the customer.
Hot Tags: two componment polyether based polyurethane prepolyer, China, manufacturers, factory, buy, Zinc Borate 2335 80, Two Componment MDI Based Polyurethane Prepolyer, MDI System Casting PU Elastomer, Flame Retardent Zinc Borate, Two Componment Polyether Based Polyurethane Prepolyer, PU Elastomer Finished Product
[[ProKeywords]]You Might Also Like
-

High Performance Pcl (Polycaprolactone) Based Castin...
-

Factory Supply CAS 11113-50-1 Boric Acid Chunks /Bor...
-

Hydroquinone Bis (2-hydroxyethyl) Ether Hqee CAS No....
-

Electric Type Large Flow Elastomer Casting Machine P...
-

Polyurethane Roller Making Machine /PU Roller Making...
-

Top Surface Layer Is a Combination of Colored EPDM G...