Polyester Polyol for CPU Used in Elastomers and The Field of Casting Polyurethane Elastomers
The same raw materials can be produced with different hardness by adjusting the A/B/C component ratio, and the raw materials need not be replaced in the hardness switching process.
Product Introduction
Our company is a high-tech enterprise specializing in R&D and production of Zinc Borate 2335 200, PTMEG Based Casting Polyurethane Prepolymer, MDI System Casting PU Elastomer. We have strong independent innovation capabilities, and our product design capabilities and manufacturing capabilities are in a leading position in the industry. No matter where you are, you can feel the fast and excellent service of our professional and technical personnel. After years of development, our business has spread all over the world. In line with the corporate philosophy of 'ethics-oriented, honesty in the world' and the work purpose of 'solving problems for customers', we will continue to provide customers with high-quality products and perfect services, and welcome your visit and guidance!
Three componment MDI system PU Prepolymer
1. Characteristics of MDI raw materials
The same raw materials can be produced with different hardness by adjusting the A/B/C component ratio, and the raw materials need not be replaced in the hardness switching process.
1) Need catalyst intervention
MDI three-component feedstock belongs to semi-prepolymer, and the reaction rate of-0H is less than that of-NH2. In order to obtain better physical properties and production efficiency, catalyst is needed
2) Environmental protection
The vapor pressure of MDI is much lower than that of TDI, and it has aromatic odor and little toxicity in the production process, so MDI is a new material that meets the needs of environmental protection.
2. Advantages of the MDI three-component series
* Adjustable hardness: the same grade of three-component raw materials can be replaced by permutation and combination to produce products with different hardness.
* Environmental protection: MDI vapor pressure is lower.
* Low equipment energy consumption: The application temperature of MDI products is lower, and the equipment energy consumption is greatly reduced.
* High production efficiency: The intervention of the catalyst makes the production efficiency of MDI products higher than that of TDI products, with low energy consumption and high efficiency.
Specifications
Item | Standard | Unit | Hardness | |||||||
60A | 65A | 70A | 75A | 80A | 85A | 90A | 95A | |||
HJ33M-A | - | g | 100 | 100 | 100 | 100 | 100 | 100 | 100 | 100 |
HJ33M-B | - | g | 224 | 184 | 144 | 124 | 104 | 84 | 69 | 56 |
HJ33M-C | - | g | 7.25 | 9.05 | 10.85 | 11.75 | 12.65 | 13.55 | 14.20 | 14.80 |
Catalyst | - | ‰ | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 |
HJ33M-A temperature | - | ℃ | 45-50 | |||||||
HJ33M-B temperature | - | ℃ | 65-75 | |||||||
HJ33M-C temperature | - | ℃ | 35-40 | |||||||
Die temperature | - | ℃ | 100-110 | |||||||
Post-maturing conditions | - | h/℃ | (12-24)/100 according to product size | |||||||
Gel time | - | mins | 7~10 | 7~10 | 7~10 | 5~7 | 5~7 | 3~5 | 3~5 | 3~5 |
Demoulding time | - | mins | 40 | 40 | 40 | 30 | 30 | 30 | 30 | 30 |
Tensile strength | GB/T528-2009 | Mpa | 35-37 | 36-38 | 36-38 | 38-40 | 38-43 | 42-47 | 43-48 | 47-52 |
100% modulus | GB/T528-2009 | Mpa | 1—2 | 2—3 | 2—3 | 2—4 | 3—5 | 5—7 | 6—8 | 8—10 |
300% modulus | GB/T528-2009 | Mpa | 2—4 | 5—8 | 7—9 | 9—12 | 11—14 | 13—16 | 14—17 | 17—20 |
Elongation at break | GB/T528-2009 | % | 551-654 | 532-637 | 522-625 | 522-623 | 481-582 | 432-535 | 422-525 | 425-527 |
Tear strength | GB/T529-2008 | KN/m | 36-44 | 42-54 | 52-63 | 61-73 | 71-82 | 81-92 | 92-104 | 104-120 |
Rebound | GB/T1681-2009 | % | 51-52 | 50-52 | 50-52 | 49-51 | 48-50 | 45-47 | 43-45 | 41-43 |
Density (25 ℃) | GB/T533-2008 | g/cm2 | 1.21 | 1.21 | 1.22 | 1.22 | 1.22 | 1.23 | 1.24 | 1.24 |
DIN drum wear | GB/T9867-2008 | mm3 | ≤40 | ≤40 | ≤38 | ≤38 | ≤38 | ≤38 | ≤35 | ≤35 |
Our Polyester Polyol for CPU Used in Elastomers and The Field of Casting Polyurethane Elastomers are well received by customers in various industries, and most of the customers who have served have become our old customers. Our company is rich in products, quality in the international leading level. We promise high-quality products, reasonable prices, and satisfactory service!
Hot Tags: three componment mdi system casting polyurethane, China, manufacturers, factory, buy, PU Square Pad, PU Tube and Pipe, PU Elastomer Finished Product, Zinc Borate 2335 80, MDI Two Componment Polyester Type Casting PU, 3 Crystal Water Zinc Borate
[[ProKeywords]]You Might Also Like
-

High Performance Pcl (Polycaprolactone) Based Castin...
-

Two Component Polyurethane Mdi Based Sport Court Syn...
-

High Quality Hydroquinone Bis (2-hydroxyethyl) Ether...
-

Black Custom Gel Wrist Rest Mouse Pads with Hand Rest
-

3D Electric Best Full Body Deep Tissue Back Shiatsu ...
-

Red Blue Black White Transparent Pneumatic PU Polyet...