Reanin-K2000 Portable Pneumatic Polyurethane Foam Spray Wall Thermal Insulation Injection Spraying Casting Coating Machine
The same raw materials can be produced with different hardness by adjusting the A/B/C component ratio, and the raw materials need not be replaced in the hardness switching process.
Product Introduction
With our professionalism in the business of MDI System Casting PU Elastomer, Quazi MDI Three Componment Casting PU, PU Square Pad, we have continuously achieved exciting results. Adhering to the business philosophy of 'customer first, forge ahead', excellent quality and perfect service are our constant promise. Relying on our strong production capacity and sales capacity, we believe that this year will be a major milestone in the development of our company. The company is committed to achieving a better life for employees and creating safe and high-quality products for customers. We deeply explore the shining points in each employee and give full play to the strengths of each employee. We have advanced production lines and testing equipment, adhering to the principle of quality first, customer first, and strive to achieve mutual benefit and win-win situation.
Three componment MDI system PU Prepolymer
1. Characteristics of MDI raw materials
The same raw materials can be produced with different hardness by adjusting the A/B/C component ratio, and the raw materials need not be replaced in the hardness switching process.
1) Need catalyst intervention
MDI three-component feedstock belongs to semi-prepolymer, and the reaction rate of-0H is less than that of-NH2. In order to obtain better physical properties and production efficiency, catalyst is needed
2) Environmental protection
The vapor pressure of MDI is much lower than that of TDI, and it has aromatic odor and little toxicity in the production process, so MDI is a new material that meets the needs of environmental protection.
2. Advantages of the MDI three-component series
* Adjustable hardness: the same grade of three-component raw materials can be replaced by permutation and combination to produce products with different hardness.
* Environmental protection: MDI vapor pressure is lower.
* Low equipment energy consumption: The application temperature of MDI products is lower, and the equipment energy consumption is greatly reduced.
* High production efficiency: The intervention of the catalyst makes the production efficiency of MDI products higher than that of TDI products, with low energy consumption and high efficiency.
Specifications
Item | Standard | Unit | Hardness | |||||||
60A | 65A | 70A | 75A | 80A | 85A | 90A | 95A | |||
HJ33M-A | - | g | 100 | 100 | 100 | 100 | 100 | 100 | 100 | 100 |
HJ33M-B | - | g | 224 | 184 | 144 | 124 | 104 | 84 | 69 | 56 |
HJ33M-C | - | g | 7.25 | 9.05 | 10.85 | 11.75 | 12.65 | 13.55 | 14.20 | 14.80 |
Catalyst | - | ‰ | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 | 1~3 |
HJ33M-A temperature | - | ℃ | 45-50 | |||||||
HJ33M-B temperature | - | ℃ | 65-75 | |||||||
HJ33M-C temperature | - | ℃ | 35-40 | |||||||
Die temperature | - | ℃ | 100-110 | |||||||
Post-maturing conditions | - | h/℃ | (12-24)/100 according to product size | |||||||
Gel time | - | mins | 7~10 | 7~10 | 7~10 | 5~7 | 5~7 | 3~5 | 3~5 | 3~5 |
Demoulding time | - | mins | 40 | 40 | 40 | 30 | 30 | 30 | 30 | 30 |
Tensile strength | GB/T528-2009 | Mpa | 35-37 | 36-38 | 36-38 | 38-40 | 38-43 | 42-47 | 43-48 | 47-52 |
100% modulus | GB/T528-2009 | Mpa | 1—2 | 2—3 | 2—3 | 2—4 | 3—5 | 5—7 | 6—8 | 8—10 |
300% modulus | GB/T528-2009 | Mpa | 2—4 | 5—8 | 7—9 | 9—12 | 11—14 | 13—16 | 14—17 | 17—20 |
Elongation at break | GB/T528-2009 | % | 551-654 | 532-637 | 522-625 | 522-623 | 481-582 | 432-535 | 422-525 | 425-527 |
Tear strength | GB/T529-2008 | KN/m | 36-44 | 42-54 | 52-63 | 61-73 | 71-82 | 81-92 | 92-104 | 104-120 |
Rebound | GB/T1681-2009 | % | 51-52 | 50-52 | 50-52 | 49-51 | 48-50 | 45-47 | 43-45 | 41-43 |
Density (25 ℃) | GB/T533-2008 | g/cm2 | 1.21 | 1.21 | 1.22 | 1.22 | 1.22 | 1.23 | 1.24 | 1.24 |
DIN drum wear | GB/T9867-2008 | mm3 | ≤40 | ≤40 | ≤38 | ≤38 | ≤38 | ≤38 | ≤35 | ≤35 |
Our Reanin-K2000 Portable Pneumatic Polyurethane Foam Spray Wall Thermal Insulation Injection Spraying Casting Coating Machine design meets customers' individual needs, product production pursues the highest performance-to-price ratio, and product delivery meets the fast pace of contemporary times. Our company adheres to the business philosophy of "excellent quality, good reputation, low price, considerate and fast service and pre-sales and after-sales technical support". In terms of talent introduction, we make corresponding long and short term employment plans according to the company's long and short term strategic goals, and draw up job responsibility requirements according to different employment positions, and introduce high quality talents according to the requirements.
Hot Tags: three componment mdi system casting polyurethane, China, manufacturers, factory, buy, Polyester Type MDI System Polyurethane Elastomer, Zinc Borate 2335 400, Three Componment MDI System Casting Polyurethane, PU Tube and Pipe, PU Square Pad, Quazi MDI Three Componment Casting PU
[[ProKeywords]]You Might Also Like
-

Military/Army Bulletproof Helmet Fast Helmet with Hi...
-

High Performance PE Light Weight Bulletproof Helmet ...
-

Zinc Borate Anhydrous CAS: 12767-90-7
-

CAS 1332-07-6 Flame Retardant Zb-2335 (anhydrous, 1,...
-

Polyurethane Polymeric Mdi Isocyanate Ab Materials R...
-

Auto Windshield Glass Polyurethane PU Adhesive Glue ...