Why Is The Cup Test Required For The Production Of Polyurethane Prepolymer Products?

Jun 30, 2021

1. Observe the ratio of A and B materials

When the ratio of A and B materials is out of balance, the tear strength of free foam materials is particularly easy to observe. At this time, increase or decrease a little A, B material and then carry out the cup test, and so on, until the center of the ratio of the two is found. But sometimes it will be difficult to find the matching center. It may be caused by uneven mixing, leakage of methylene chloride (cleaning fluid), overheating and overcooling of the ambient temperature. At this time, separately test the respective flow rates of A and B materials to determine whether the flow ratio of A and B materials is normal. It should be noted that if the raw material is prevented for too long, the central value of the ratio of the polyurethane prepolymer is not the value of the standard ratio. In many cases, the amount of B material will increase, and the proportioning center needs to be searched again.


2. Detection of foaming density

Whether the free foaming density is consistent with the standard free foaming density is an important indicator to observe whether the reaction reactivity of the stock solution is normal. Too high or too low indicates that the reaction is not proceeding normally, and the gel and foaming speed are not in harmony . The difference between the free foam density and the density of the finished product cannot be too small, otherwise, if the foaming pressure is too small, the surface quality of the finished product will deteriorate. In actual production, because the foaming pressure is too small, the surface quality of the finished product will deteriorate. In actual production of polyurethane prepolymer, insufficient printing foaming pressure causes problems. For example, the commonly used PU sole stock solution generally has a free foaming density standard of about 0.25kg/cm3. The density of the finished product is 0.5~0.7g/cm3, and the difference is more than 0.25kg/cm3. If the density of the finished product is reduced to about 0.4g/cm3 in order to save materials, resulting in the difference between the two being below 0.15g/cm3, the surface quality of the PU sole at the production site will be poor.


3. Check the lotus leaf for bubbles

Sometimes, when the mixture of material A and B is poured dry, air bubbles have been brought into it. This may be caused by the imperfect sealing of the machine head and imperfect sealing of the sprayed polyurethane prepolymer. Therefore, it can be observed by self-foaming. When the new mixing head is just replaced, bubbles are prone to appear in the first few cups, but after a few more cups of experimentation. Since the source of the leak has been sealed by the mixed liquid, the situation will get better.


4. Detect the phased indicators in the automatic foaming process

The reactivity index of the automatic foam test, in addition to the strength index, there are milky white time, rise time, non-stick time, and elastic time. Check these time values.

You Might Also Like